316 Stainless Steel Polished Plate
Specification:{{0}}.5-3.0mm
Surface Treatment:Mirror, Golden Mirror, Hairline, No.4 Satin etc.
What is 316 stainless steel polished plate?
316 stainless steel polished plate (UNS S31600, 06Cr17Ni12Mo2 in GB/T 24511) is a high-end plate with a mirror effect formed by mechanical polishing or electrolytic polishing on a 316 austenitic stainless steel substrate. It contains 2-3% molybdenum (Mo) and 10-14% nickel (Ni). The surface roughness can reach Ra Less than or equal to 0.8μm (ordinary polishing) to Ra Less than or equal to 0.2μm (mirror polishing). It is widely used in medical equipment, food machinery, high-end decoration and other fields with strict requirements on corrosion resistance and appearance.
316

316 stainless steel plate
What is the difference between 316 stainless steel polishing plate and 304 polishing plate?
Corrosion resistance: 316 contains Mo, and is resistant to Cl⁻ concentration of 5000ppm (304 is 1000ppm), suitable for medium and high chlorine environments;
Cost: 316 is 20%-30% more expensive than 304, but its life is more than doubled, and it has a higher long-term cost-effectiveness.
What is the maximum operating temperature of 316 polishing plate?
Long-term use Less than or equal to 800 degree , short-term peak 900 degree , it is recommended to use high-temperature resistant 310S stainless steel (resistant to 1100 degree ) above this temperature
GNEE is a large-scale integrated processor with stainless steel coils, stainless steel strips, stainless steel plates and stainless steel pipes as its main business. The monthly shipment volume is 5,000+ tons, the standing inventory is 15,000+ tons, and the professional team is 200+ people. The company can provide corresponding certifications according to customer requirements, such as: EN, ASTM/ASME, DIN/JUV, JIS/SUS, etc.
Standard Specification Of 316 Stainless Steel Sheet
Thickness: 0.3mm-200mm
Length: 2000mm / 2438mm / 3000mm / 5800mm / 6000mm / 12000mm, etc.
Width: 40mm-600mm / 1000mm / 1219mm / 1500mm / 1800mm / 2000mm / 2500mm / 3000mm / 3500mm, etc.
Surface: BA / 2B / NO.1 / NO.4 / 4K / HL / 8K, etc.
| Less than or equal to 0.8μm | ||||
| Less than or equal to 0.4μm | ISO 10993 (Medical) | |||
| Less than or equal to 1.6μm |
Manufacturer of 2B Finish Stainless Steel 316 Thin Sheet



Tag: 316 stainless steel polished plate, China 316 stainless steel polished plate manufacturers, suppliers, factory, Placa personalizada de aço inoxidável, placa de folha de aço inoxidável, Placa de grau de aço inoxidável, Função de placa de aço inoxidável, placa retangular de aço inoxidável, placa de fita de aço inoxidável
You Might Also Like
Enviar inquérito