O que é o ASTM A790 equivalente?
May 26, 2025
Deixe um recado
O que é ASTM A790?
ASTM A790 is a standard specification for seamless and welded ferritic/austenitic stainless steel pipe, also known as duplex stainless steel pipe. It is primarily used in applications requiring high strength, excellent corrosion resistance, and good weldability, such as chemical processing, oil and gas, and marine environments.
O que é o ASTM A790 equivalente?
| ASTM A790 Grade | Designação UNS | Pt / din equivalente | Nome comum |
|---|---|---|---|
| A790 S31803 / S32205 | UNS S31803 / S32205 | En 1.4462 / x2crnimon 22-5-3 | Duplex 2205 |
| A790 S32750 | UNS S32750 | En 1.4410 / x2crnimon 25-7-4 | Super Duplex 2507 |
| A790 S32760 | UNS S32760 | En 1.4501 / x2crnimocuwn 25-7-4 | Super Duplex (Zeron 100) |
| A790 S32304 | UNS S32304 | En 1.4362 / x2crnin 23-4 | Duplex enxuta 2304 |
Composição química ASTM A790

ASTM A790 Propriedades mecânicas

Qual material é ASTM A790 UNS S31803?
ASTM A890 CD3MN ou Grau 4A é o grau equivalente mais próximo do aço inoxidável super duplex forjado uns s 32205. também é designado como ASTM A995 e ASME SA351/995 CD3MN ou 4A, também escrito como J92205 ou x2crnimon {11mn {11a}} {11mon} {11mon {também 4a, como J92205 ou x2crnimon {11mon {11a} {também J92205 ou x2crnimon {11mon {11a.
O que é o material ASTM A790 UNS S32760?
Astm A790 Uns S32760 Welded Pipes have a smooth finish as they are made from cold-formed stainless steel and also have strong mechanical traits. They are resistant to chloride pitting and coercive corrosion. 18 Swg., 14 20 Swg., Swg . swg ., 12 16 swg ., 10 swg .
Qual é a diferença entre S31803 e S32205?
O S32205 possui controle de composição mais rígido e resistência aprimorada à corrosão em comparação com s 31803.